1.2344 ESR
SKU: 2343 ESR
DIN : X50CrVMo5-1
AISI/SAE : -
EXPLANATION: ESR TWICE MELTING WITH THE METHOD, EXTRA CLEANING OF THE STEEL IS PROVIDED AND THE GRAIN STRUCTURE IS FINALIZED. IT IS HOT WORK TOOL STEEL WITH HIGH Toughness and TEMP RESISTANCE. SUITABLE FOR NITRATION.
Chemical Composition
C%
Si%
mn
cr
B.C
V
0.37
1.0
0.38
5.15
1.30
0.40
Mechanical Properties
Tempering °C one hundred 200 300 400 500 550 Hardness HRC 53 52 51 52 54 53 Heat Treatment Information
Heat Treatments
Heat
Environment
Hardness
Soft Annealing
750 - 790 °C
Oven
229 HB
Stress Relief
600 - 650°C
Oven
Hardening
1000 - 1050°C
Oil - Gas - Air - Hot Bath
Tempering Curve
Physical Properties
temperature (⁰C) 20°C 350°C 700°C Thermal Conductivity ( W/ mK ) 25.3 27.2 30.5 Usage areas
- In casting molds,
- Forging dies, extrusion tools,
- In plastic manufacturing,
- In screws and sleeves,
- On hot cutting blades,
- It is used in hydroform molds.