top of page
Titanium-Zirconium-Molybdenum

Titanium-Zirconium-Molybdenum

SKU: TZM

EU:-

AISI/SAE : -

DESCRIPTION: TZM has a higher recrystallization temperature, higher strength, hardness and good at room temperature _cc781905-5cde-3194-bb358-1365 than unalloyed Molybdenum. TZM offers twice the strength of pure molybdenum at temperatures above 1300C. TZM has a recrystallization temperature of about 250°C, higher than molybdenum and offers better weldability. In addition, TZM exhibits good thermal conductivity, low vapor pressure and good corrosion resistance.

  • Chemical Composition

    Ti %

    B.C%

    Zr%

        C %

    0.4-0.55

    Balance

    0.06-0.12

    0.01-0.04

  • Usage areas

    • In arc chamber parts of ion providers.
    • In structures of high temperature furnaces.
    • In Casting Molds.